Find speed for two hours with hss tools, Mechanical Engineering

Assignment Help:

Find speed for two hours with HSS tools

Find speed for two hours tool life for dry machining of free cutting mild steel with HSS tool.

Solution

From Table 3, a value of C = 74 m/min is chosen while for HSS tool a mean value of n = 0.125 has been assumed.

V tn = C

V = C /t n

=  74 /1200.125

= 74 /1.82

= 40.67

= 40.67 metres/minute

Table 3: Constant C for Taylor's Equation

990_Tool Life Equation 1.png


Related Discussions:- Find speed for two hours with hss tools

Difference between von mises and maximum principal stress, What is the diff...

What is the difference between von-mises and maximum principal stress? What is axisymmetric, plane stress, and plane strain modeling? What is difference between a beam, spar,

What do you mean by extrusion, Q. What do you mean by extrusion? • Ex...

Q. What do you mean by extrusion? • Extrusion is a process used to create objects of a fixed cross-sectional profile. A material is pushed or drawn through a die of the desir

Find the speed of shaft , Find the speed of shaft : Find the speed of...

Find the speed of shaft : Find the speed of shaft driven with the belt by an engine running at 600 rotation per minute. The thickness of belt is 2cm, diameter of engine pulle

Maximal conductances and reversal potentials, By introducing their model of...

By introducing their model of neural excitability in 1952, Alan Lloyd Hodgkin and Andrew Huxley not only shed light on the mechanism underlying a very important phenomenon in Physi

Otto cycle - thermodynamics, Ott o Cycle (1876): This cycle consists...

Ott o Cycle (1876): This cycle consists of the two reversible adiabatic processes and the two constant volume processes as shown in the figure given below on P - V and T -

Assignemnt , A heating section consists of a 10 in diameter duct which hous...

A heating section consists of a 10 in diameter duct which houses a 8 kW electric resistance heater. Air enters the heating section at 14.7 psia 40oF, and 35 percent relative humidi

Submerged arc welding, Submerged Arc Welding   Single pass filler we...

Submerged Arc Welding   Single pass filler welds upto (8.0 mm) maximum and groove welds made with a single pass or a single pass each side, may be made using an E7os-x elect

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd