Define the cavitation - underwater inspection of bridge, Civil Engineering

Assignment Help:

Define the Cavitation - underwater inspection of bridge?

Cavitation damage is caused by repeated impact forces caused by collapse of vapour bubbles in rapidly flowing water. The appearance of concrete damaged by cavitation is generally different from that damaged by abrasion erosion. Instead of a smooth, worn appearance, the concrete will appear very rough and pitted. In severe cases, cavitation may remove large quantities of concrete and may endanger the structure. Usually cavitation occurs as a result of water velocities greater than 12 m/sec.


Related Discussions:- Define the cavitation - underwater inspection of bridge

Determine the crash rate - transportation, A five-mile long section of two-...

A five-mile long section of two-lane road has an AADT of 8,000.  There have been six crashes on this section of road during the past two years.  What is the crash rate? R sec

Settlement due to increasing load on surrounding soil, Q. Settlement due to...

Q. Settlement due to Increasing Load on Surrounding Soil? When any portion of the ground surface  has been loaded, it causes  the surface  of adjacent soil also to tilt and set

Define structural damage - underwater inspection of bridge, Define Structur...

Define Structural Damage - underwater inspection of bridge? Structural damage to the substructure below waterline can be classified as under: i. Construction damage or error

Determine the head loss due to friction, Determine the head loss due to fri...

Determine the head loss due to friction using the Darcy-Weisbach equation. The water is pumped at 3.0 gallons per minute, has a temperature of 60 °F and is pumped through a 1inch s

What is specific energy - hydrologic system, What is Specific Energy Ap...

What is Specific Energy Applying the Bernoulli energy equation in open channel flow results in Z = 0 (channel bottom or datum), the pressure head (p/γ) = d, and the velocity he

Sealing moving cracks and non-moving cracks, Sealing moving cracks and non-...

Sealing moving cracks and non-moving cracks In developing a suitable method to seal up cracks detected on concrete surface, it's of paramount importance to conclude if further

Trigo, a pilot entering a bay on course

a pilot entering a bay on course

Concrete, whats the role of gypsum in concrete?

whats the role of gypsum in concrete?

Theodolite, definion of local attraction and correction

definion of local attraction and correction

Amount of water that added to achieve the optimum moisture, Geotechnical pr...

Geotechnical project specifications require that the soil's optimum moisture content of 24% be maintained during the roadbed's construction.   The field moisture test finds that fi

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd