Explain planar defects, Chemical Engineering

Assignment Help:

Planar defects

* Grain boundaries occur where the crystallographic direction of the lattice abruptly changes. This usually happens when two crystals start growing separately and then meet.

* Anti phase boundaries happen in ordered alloys: in this case, the crystallographic direction remains the same, every side of the boundary has an  opposite phase: For example if the ordering is usually ABABABAB, an anti phase boundary takes the form of ABABBABA.

 


Related Discussions:- Explain planar defects

Explain positive and negative photo resist, Positive and Negative Photo res...

Positive and Negative Photo resist There are two types of photo resist: positive and negative. For positive resists, the resist is exposed with UV light where the underlying ma

Valves, Describe different type of valves

Describe different type of valves

Ammonia, full process of ammonia synthesis

full process of ammonia synthesis

Look, when do the cell get alot of thing in there thing because am confuse ...

when do the cell get alot of thing in there thing because am confuse cause is alot of thing becaus is crazy

Chemical reaction, the chemical reaction taking place in the kiln?

the chemical reaction taking place in the kiln?

Moment, the frame in figure consisted of members AB and BCD connected by pi...

the frame in figure consisted of members AB and BCD connected by pin at B, and member AB is a quarter circle of radius 75mm. the whole frame is supported by pins at A and C. for th

Water treatment, concequence of sludge and slag formation in boiler

concequence of sludge and slag formation in boiler

Write Your Message!

Captcha
Free Assignment Quote

Assured A++ Grade

Get guaranteed satisfaction & time on delivery in every assignment order you paid with us! We ensure premium quality solution document along with free turntin report!

All rights reserved! Copyrights ©2019-2020 ExpertsMind IT Educational Pvt Ltd